Pressure sensitive adhesive formula

formula

Component dosage /g component dosage /g
Polyisobutylene rubber 100 Petroleum ether Appropriate terpene resin 80


Preparation and curing into 20%, 30% two kinds of glue. After gluing, let dry for 5 to 10 minutes.

Use This glue uses a temperature of -40 ~ +50 °C, used for bonding polyethylene, polypropylene, polyester film and all kinds of metal foil, but also for polyester, aluminum foil, nameplates and other bonding.